Density & Weight
| Egenskap |
Värde |
Enhet |
Teststandard |
| Density |
2.1 |
g/cm³ |
ASTM D1457 |
Tensile Properties
| Egenskap |
Värde |
Enhet |
Teststandard |
| Tensile Strength |
22 |
MPa |
ASTM D4894 |
| Modulus of elasticity (tensile) |
750 |
MPa |
ISO 527 |
| Breakdown Voltage |
18 |
MPa |
ASTM D1457 |
| Break Elongation |
300 |
% |
ASTM D1457 |
Flexural Properties
| Egenskap |
Värde |
Enhet |
Teststandard |
| Flexural Strength |
6 |
MPa |
ISO 178 |
Impact Resistance
| Egenskap |
Värde |
Enhet |
Teststandard |
| Notched impact strength (Charpy) |
16 |
kJ/m² |
ISO 179 |
Hardness
| Egenskap |
Värde |
Enhet |
Teststandard |
| Hardness Shore D |
58.5 |
° Shore D |
ASTM D1706 |
| Ball pressure hardness |
45 |
MPa |
ISO 2039 |
Temperature Limits
| Egenskap |
Värde |
Enhet |
Teststandard |
| Maximal operating temperature (short-term) |
260 |
°C |
|
| Maximum Operating Temperature |
260 |
°C |
|
| Minimum temperature |
-200 |
°C |
|
Insulation Properties
| Egenskap |
Värde |
Enhet |
Teststandard |
| Volume Resistivity |
104 |
Ω·cm |
ASTM D257 |
Tillgängliga dokument för nedladdning: