Density & Weight
| Egenskap |
Värde |
Enhet |
Teststandard |
| Density |
3 |
g/cm³ |
DIN EN ISO 1183-1 |
Moisture Absorption
| Egenskap |
Värde |
Enhet |
Teststandard |
| Water absorption to saturation |
0.1 |
% |
DIN EN ISO 62 |
Tensile Properties
| Egenskap |
Värde |
Enhet |
Teststandard |
| Tensile Strength |
53 |
MPa |
DIN EN ISO 527-2 |
| Modulus of elasticity (tensile) |
3000 |
MPa |
DIN EN ISO 527-2 |
| Break Elongation |
8 |
% |
DIN EN ISO 527-2 |
Flexural Properties
| Egenskap |
Värde |
Enhet |
Teststandard |
| Flexural Strength |
53 |
MPa |
DIN EN ISO 527-2 |
Impact Resistance
| Egenskap |
Värde |
Enhet |
Teststandard |
| Notched impact strength (Charpy) |
25 |
kJ/m² |
DIN EN ISO 179-1 |
| Impact Resistance (Charpy) |
2 |
kJ/m² |
DIN EN ISO 179-1 |
Hardness
| Egenskap |
Värde |
Enhet |
Teststandard |
| Hardness Shore D |
81 |
° Shore D |
DIN EN ISO 868 |
Temperature Limits
| Egenskap |
Värde |
Enhet |
Teststandard |
| Melting point |
179 |
°C |
DIN EN ISO 11357 |
| Maximal operating temperature (short-term) |
150 |
°C |
|
| Maximum Operating Temperature |
110 |
°C |
|
| Heat deflection temperature (HDT/A) |
141 |
°C |
|
| Vicat softening temperature (VST/B/50) |
90 |
°C |
DIN EN ISO 306 |
Thermal Conductivity
| Egenskap |
Värde |
Enhet |
Teststandard |
| Thermal Conductivity |
0.46 |
W/(m·K) |
ISO 22007-4 |
Thermal Expansion
| Egenskap |
Värde |
Enhet |
Teststandard |
| Thermal Expansion Coefficient |
23 |
10⁻⁴/K |
DIN EN ISO 11359-1 |
Insulation Properties
| Egenskap |
Värde |
Enhet |
Teststandard |
| Dielectric Strength |
23 |
kV/mm |
ISO 60243-1 |
| Volume Resistivity |
1014 |
Ω |
DIN EN 62631-3-1 |
| Dielectric Constant (1 MHz) |
2.4 |
- |
IEC 60250 |
Static spread
| Egenskap |
Värde |
Enhet |
Teststandard |
| Surface Resistivity |
1014 |
Ω |
DIN EN 62631-3-2 |
Fire Classification
| Egenskap |
Värde |
Enhet |
Teststandard |
| Flammability Classification (UL 94) |
60695 |
|
UL 94 |
Tillgängliga dokument för nedladdning: